Welding Electrode

ROYAL CHROM – 9 (SPL) (E 9015 B9)

AWS : SFA 5.5, E 9015 B9 EN ISO 3580 A E CrMo 9 1 B 32 H5

Applications

It is used for welding of 9% Cr, plates, pipes, tubes. It is also used for welding of 7 to 10% Cr, 1% Mo steel for general
corrosion and heat resistance application. Surfacing of turbine Blades, Valve, Seats, Pump parts etc. A 213- T9 Tube , A335- P9 Pipe , P11&,A387

Packing

Vaccum packing

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Preheat at 150 – 250 °C and postheat at 740 ± 15 °C.
2) Dry the electrode at 250 – 300 °C for 60 Min- before use.

Chemical Composition Of Weld Metal

C%Mn%Si%S%P%Cr%Ni%Mo%
0.080 – 0.131.20 Max0.30 Max0.010 Max0.010 Max8.0 – 10.500.80 Max0.85 – 1.20

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)Y.S.(N/mm²)ELONGATION ( L = 4d ) %
620 Min530 Min17 % Min

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONCurrent (Amps)In Amps
2.50 X 350210DC (+)60 – 90
3.15 X 350210100-140
4.00 X 350210140-180
5.00 X 350210180-230

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS : A / SFA 5.11, E Ni Cu - 7 EN ISO 1472 A E Ni 4060

Share On:

Enquiry form

ROYAL CHROM – 9 (SPL) (E 9015 B9)

AWS : SFA 5.5, E 9015 B9 EN ISO 3580 A E CrMo 9 1 B 32 H5

Contact Form

×

Hello!

Click one of our contacts below to chat on WhatsApp

×