It is used for welding of 5% Cr, 0.5% Mo steel for high temp application in oil refeneries. Power plants, Petrochemical plants. Fertilizer Industries.
1G 2F 3G 4G
1) Preheat at 150 – 250 °C and postheat at 690 ± 14 °C.
2) Dry the electrode at 250 – 300 °C for 60 Min- before use.
C% | Mn% | Si% | S% | P% | Cr% | Ni% | Mo% |
---|---|---|---|---|---|---|---|
0.05 – 0.10 | 1.0 Max | 0.90 Max | 0.030 Max | 0.030 Max | 4 .0 – 6.0 | 0.40 Max | 0.45 – 0.65 |
U.T.S.(N/mm²) | Y.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|---|
550 Min | 460 Min | 19 % Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | Current (Amps) | In Amps |
---|---|---|---|---|
2.50 X 350 | 5 | 20 | DC (+) | 60 – 90 |
3.15 X 350 | 5 | 20 | 100-140 | |
4.00 X 350 | 5 | 20 | 140-180 | |
5.00 X 350 | 5 | 20 | 190-240 |