For welding 0.9% N & 0.5 Mo steel Suitable for welding of manganese molly steel. Low alloy high tensile boiler tubes & boiler Plates etc.
1G 2F 3G 4G
1) Dry the electrode a 250 – 300°C for 60 Min- before use .
2) Preheat at 100 – 200 °C &post heat at 620 ± 15 °C Keep the arc as short as
possible.
C% | Mn% | Si% | S% | P% | Cr% | Mo% |
---|---|---|---|---|---|---|
0.12 Max | 1.0-1.75 | 0.80 | 0.030 Max | 0.030 Max | 0.90 Max | 0.25-0.45 |
U.T.S.(N/mm²) | Y.S.(N/mm²) | ELONGATION ( L = 4d ) % | IMPACT (CVN) AT – 50° C ( J) |
---|---|---|---|
560 – 660 | 460 – 570 | 19 % | 27 Joules Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | Current (Amps) | In Amps |
---|---|---|---|---|
2.50 X 350 | 5 | 20 | AC/DC (+) | 70 – 100 |
3.15 X 350 | 5 | 20 | 90-130 | |
4.00 X 350 | 5 | 20 | 140-180 | |
5.00 X 350 | 5 | 20 | 180-220 |