ROYAL THERM- 90 D (E 9018 –D3)

AWS: SFA 5.5, E 9018 –D3 IS : 1395: E 63BD 1241

Applications

Welding of grain rened steels. Q&T steel, HSLA steel, structural fabrication, Penstocks, Tanks, pressure vessels.

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Dry the electrode a 250 – 300°C for 60 Min- before use .
2) Preheat at 100 – 200 °C & post heat at 620 ± 15 °C
3) Keep the arc as short aspossble.

Chemical Composition Of Weld Metal

C%Mn%Si%S%P%Cr%Mo%
0.12 Max1.0-1.750.800.030 Max0.030 Max0.90 Max0.25-0.45

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)Y.S.(N/mm²)ELONGATION ( L = 4d ) %IMPACT (CVN) AT – 50° C ( J)
620 Min530 Min22 % Min50 Joules

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONCurrent (Amps)In Amps
2.50 X 350520AC/DC (+)70 – 100
3.15 X 350520100-140
4.00 X 350520140-180
5.00 X 350520180-230

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS : SFA 5.5, E 7018 B2L EN ISO 3580 A E CrMo 1 L B 32 H5
AWS: SFA 5.11, E Ni -1 EN ISO 14172 A E Ni 2061