A unique electrode for cold welding of cast iron without preheat and for joining cast iron to mild steel. Also suitable for surfacing cast iron parts subject ot erosion, corrosion and high temperatures. Best suited for repairing intricate cast iron
parts, water pumps housing, Electric motor bodies and covers, Machine frames, Cylinder blocks, gears, also ideal for
salvaging foundry castings, Gears box and differential housings, lathe beds,
1G 2F 3G 4G 5G
1) Clean the welding zone and check the surface for cracks and defects, use a short arc with low current ot deposit a string bead
not exceeding 50 mm
2) Peen the deposit to reduce residual stresses.
U.T.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
300-340 | 130-150 Brinell |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | In Amps |
---|---|---|---|
2.50 X 350 | 2 Kg | 10 Kg | 40-70 |
3.15 X 350 | 2 Kg | 10 Kg | 60-110 |
4.00 X 350 | 2 Kg | 10 Kg | 80-120 |
5.00 X 350 | 2 Kg | 10 Kg |