For the fabrication of chemical plants. Paper mill equipments Pickling plant etc., Joining and surfacing of similar composition of stainless steel.
1G 2F 3G 4G
Vaccum Pack
1) Dry the electrode at 350°C for 60 Min- before use .
2) Keep the arc as short as possible.
3) Remove rust,water,oiland paint from the surface to be welded.
C% | Mn% | Si% | S% | P% | Cr% | Ni% | Mo% | Nb(Cb)% |
---|---|---|---|---|---|---|---|---|
0.080 Max | 0.50 – 2.50 | 1.00 Max | 0.030% | 0.040% | 17.0 – 20.0 | 11.0 – 14.0 | 2.0 – 2.50 | 0.50 – 1.0 |
U.T.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
550 Min | 25% Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | Current (Amps) | In Amps |
---|---|---|---|---|
2.50 X 350 | 2 | 10 | AC / DC (+) | 60 – 80 |
3.20 x 350 | 2 | 10 | 80 – 100 | |
4.00 x 350 | 2 | 10 | 110 – 140 | |
5.00 x 350 | 2 | 10 | 140 – 180 |