Welding Electrode

ROYAL CHROME – 13 / 4 (E 410 – 15 NiMoX)

SFA 5.4 AWS E 410 – 15 NiMoX EN ISO 3581 A E 13 4 B 22

Applications

Welding and surfacing of Turbines, Armature, Valves, Pumps. Welding for similar composition of casting steel. Welding of martenistic / ferritic stainless steel of 13% Cr, 4% Ni.

Welding Positions

1G 2F 3G 4G

Packing

Vaccum packing

Notes On Usage

1) Preheat the job at 150-200°C & PWHT. at 595 – 620oC for one hour soaking
2) keep the current as low as possible
3) Remove dirts such as oil and dust from the groove.
4) Dry the electrodes at 350oC for 60 minute before use

Chemical Composition Of Weld Metal

C%Mn%Si%S%P%Cr%Ni%Mo%
0.06 Max1.00 Max0.90 Max0.030 Max0.040 Max11.0 – 12.504.0 – 5.00.40 – 0.70

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)ELONGATION ( L = 4d ) %
76015

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONCurrent (Amps)In Amps
2.50 X 350210DC (+)60 – 80
3.15 x 35021080 – 120
4.00 x 350210110 – 160
5.00 x 350210150 – 190

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS A/SFA 5.15, Est. EN ISO 1071 A EC Fe 1 3

Share On:

Enquiry form

ROYAL CHROME – 13 / 4 (E 410 – 15 NiMoX)

SFA 5.4 AWS E 410 – 15 NiMoX EN ISO 3581 A E 13 4 B 22

Contact Form

×

Hello!

Click one of our contacts below to chat on WhatsApp

×