Welding Electrode

ROYAL CHROME – 13 (E 410 – 15)

SFA 5.4 AWS E 410 - 15 EN ISO 3581 A E 13 B 22

Applications

Turbines, armature valves & pumps.

Welding Positions

1G 2F 3G 4G

Packing

Vaccum packing

Notes On Usage

1) Preheat the job at 150-200oC & PWHT. at 730 – 760oC for one hour soaking
2) keep the current as low as possible
3) Remove dirts such as oil and dust from the groove.

Chemical Composition Of Weld Metal

C%Mn%Si%S%P%Cr%Ni%Mo%
0.12 Max1.00 Max0.90 Max0.030 Max0.040 Max11.0 – 13.50.70 Max0.75 Max

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)Y.S(N/mm²)ELONGATION ( L = 4d ) %
520 Min470 Min20% Min

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONCurrent (Amps)In Amps
2.50 X 350210DC (+)60 – 80
3.15 x 35021080 – 100
4.00 x 350210100 – 140
5.00 x 350210140 – 180

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS / SFA 5.11 E NiCrMo – 3 EN ISO 14172 A E Ni 6625