Suitable for welding steel containing 22 – 26% and 11 – 14 % Ni, 2 – 3 % Mo also for joints between 18 Cr – 8 Ni stainless steel and mild steel or low alloy steel.
1G 2F 3G 4G
Vaccum Pack
1) Dry the electrode a 350°C for 60 Min- before use.
2) Keep the arc as short as possible.
3) Use currents as low as possible to avoid excessive dilution.
C% | Mn% | Si% | S% | P% | Cr% | Ni% | Mo% |
---|---|---|---|---|---|---|---|
0.12 Max | 0.50 – 2.50 | 1.00 Max | 0.030 Max | 0.040 Max | 22.0 – 25.0 | 12.0 – 14.0 | 2.0 – 3.0 |
U.T.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
550 | 30 % Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | LBS PER PACKET | LBS PER CARTON | In Amps | Current (Amps) |
---|---|---|---|---|---|---|
2.50 X 350 | 2 | 10 | 4.40 | 22.05 | 45 – 85 | AC/DC (+) |
3.20 x 350 | 2 | 10 | 4.40 | 22.05 | 85 – 115 | |
4.00 x 350 | 2 | 10 | 4.40 | 22.05 | 100 – 140 | |
5.00 x 350 | 2 | 10 | 4.40 | 22.05 | 135 – 180 |