Suitable for welding steel containing 22 – 26% Cr, 11 – 14 % Ni, 2-3% Mo, also for joints between 18 Cr, – 8 Ni, stainless steel and mild steel, or low alloy steel as well as clad steel.
1G 2F 3G 4G
Vaccum packing
1) Dry the electrodes at 350°C for 60 minute before use
2) Keep the arc as short as possible.
3) Use currents as low as possible to avoid excessive dilution.
C% | Mn% | Si% | S% | P% | Cr% | Ni% | Mo% |
---|---|---|---|---|---|---|---|
0.040 Max | 0.50- 2.50 | 1.00 Max | 0.030 Max | 0.040 Max | 22.0 – 25.0 | 12.0 – 14.0 | 2.0 – 3.0 |
U.T.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
520 Min | 30 % Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | Current (Amps) | In Amps |
---|---|---|---|---|
2.50 X 350 | 2 | 10 | AC/DC (+) | 45-85 |
3.15 x 350 | 2 | 10 | 85-115 | |
4.00 x 350 | 2 | 10 | 100-145 | |
5.00 x 350 | 2 | 10 | 135-180 |