Recommended for AISI 309 grade of stainless steel and straight chrome steel for joining clad steel, low alloy steel and carbon steel.
B.V.
Vaccum packing
1G 2F 3G 4G
1) Dry the electrode a 350°C for 60 Min- before use.
2) Keep the arc as short as possible.
U.T.S.(N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
540 | 30 % Min |
SIZE ( mm ) | KG PER PACKET | KG PER CARTON | Current (Amps) | In Amps |
---|---|---|---|---|
2.50 X 350 | 2 | 10 | AC/DC (+) | 45-85 |
3.15 X 350 | 2 | 10 | 85 -115 | |
4.00 X 350 | 2 | 10 | 100 -140 | |
5.00 X 350 | 2 | 10 | 135 – 180 |