Welding Electrode

ROYAL THERM – 100M (E 10018M)

E 10018M

SFA 5.5 AWS E 10018M

Applications

Welding of high tensile steel such as USS – T – 1. Welding of Penstocks, Earth moving equipment’s. Heavy duty structural steel, fabrication for High Tensile Steel.

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Dry the electrode at 250 – 300 °C for 60 Min- before use.
2) Keep the arc as short as possible.

Chemical Composition Of Weld Metal

C% Mn% Si% S% P% Cr% Ni% Mo%
0.10 Max 0.75 – 1.70 0.60 Max 0.030 Max 0.030 Max 0.35 Max 1.40 – 2.10 0.25 – 0.50

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²) Y.S.(N/mm²) ELONGATION ( L = 4d ) % IMPACT ( CVN ) AT – 50 o C ( J )
690 Min 600 Min 16 % Min 27 Joules Min

Packing and Welding Current

SIZE ( mm ) KG PER PACKET KG PER CARTON Current (Amps) In Amps
2.50 X 350 5 20 AC/DC (+) 80 – 100
3.15 X 350 5 20 100-140
4.00 X 350 5 20 140-180
5.00 X 350 5 20 180-230

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS: SFA 5.11, E NiCrMo-6 EN ISO 14172 A E Ni 6620