Welding Electrode

ROYAL – 7016 (E 7016)

E 7016

AWS : A 5.1, E 7016

Applications

For joining Mild Steel to Cast Iron, For Butt Welding on Rail Ends & Railway Class III Steels, For xing Rails to Mild Steel Girders for Overhead Cranes.

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Dry the electrode at 300-350 °C for 60 min.before use.
2) Adopt back step method or strike the arc on a small steel plate prepared for this particular pupose to prevent blow hole at the arc starting.
3) Keep the arc as short as possible.

Chemical Composition Of Weld Metal

C% Mn% Si% S% P% Cr% Ni% Mo%
0.15 Max 1.60 Max 0.75 Max 0.035 Max 0.035 Max 0.20 Max 0.30 Max 0.30 Max

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²) Y.S.(N/mm²) ELONGATION( L = 4d ) % IMPACT (CVN) AT – 30° C ( J ) Hydrogen content in 100grm weld metal
490 Min 400 Min 22 % Min 27 Joules Min 5 ml Max

Packing and Welding Current

SIZE ( mm ) KG PER PACKET KG PER CARTON Current (Amps) In Amps
2.50 x 350 5 20 AC (OCV 70) /DC (+) 60-95
3.15 x 350 5 20 90-120
4.00 x 350 5 20 140-190
5.00 x 350 5 20 190-250
6.30 x 450 5 20 250-310