Welding Electrode

Applications

ideally suited for joining and building up for low and medium carbon steels. Equally good for depositing buffer layers before hard facing pressure vessels ,steel casting , vehicle chassis etc.

Welding Positions

1G 2F 3G 4G 5G

Notes on Usage

1) To, get best results dry the electrodes at 250 oC for about 2 hours before use.
2) Cleaning the weld area is must to achieve good results.

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)ELONGATION ( L = 4d ) %
600 Min22 – 30

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONIn Amps
2.50 X 3502 Kg10 Kg60 – 90
3.15 X 3502 Kg10 Kg90 – 140
4.00 X 3502 Kg10 Kg120 – 160
5.00 X 3502 Kg10 Kg180 – 250

Related Products

AWS : A / SFA 5.11, E Ni Cu - 7 EN ISO 1472 A E Ni 4060
AWS A/SFA 5.15, Est. EN ISO 1071 A EC Fe 1 3
AWS: SFA 5.11, E NiCrFe-3 EN ISO 14172 A E Ni 6182