Welding Electrode

ROYAL 2209 (E 2209 -16)

E 2209 -16

AWS / SFA 5.4 E 2209 -16 EN ISO 3581 A E 22 9 3 N

Applications

It is used for welding of duplex stainless steel material were the weld metal deposited combines increase tensile strength with improve resistance to pitting corrosive.

Packing

Vaccum Pack

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Dry the electrodes at 350° C for 60 min. before use.
2) Keep the current as low as possible.
3) Remove rust, water, oil, paint etc. from groove.

Chemical Composition Of Weld Metal

C% Mn% Si% S% P% Cr% Ni% Mo% Cu% N%
0.040Max 0.50– 2.00 1.00 Max 0.030 Max 0.040 Max 22.5 –23.5 8.5 – 10.5 2.5-3.50 0.75Max 0.08- 0.20

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²) ELONGATION ( L = 4d ) %
690 20-28

Packing and Welding Current

SIZE ( mm ) KG PER PACKET KG PER CARTON LBS PER PACKET LBS PER CARTON In Amps Current (Amps)
2.50 X 350 2 10 4.40 22.05 50 – 90 AC/DC (+)
3.20 x 350 2 10 4.40 22.05 90 – 140
4.00 x 350 2 10 4.40 22.05 120 – 170
5.00 x 350 2 10 4.40 22.05 180 – 220

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS: SFA 5.11, E NiCrFe-2 EN ISO 14172 AE Ni 6082