Welding Electrode

ROYAL 7018 G (E 7018 G)

E 7018 G

AWS : SFA 5.5, E 7018 G EN ISO 2560 A E 42 5 Z B 32 H5

Applications

Welding of high strength steel, heavy duty structural fabrication, fine grained, Q & T steel, pressure vessels, tanks, Penstocks.

Welding Positions

1G 2F 3G 4G

Approvals

E.I.L

Notes On Usage

1) Dry the electrodes at 250 – 350°C for 60 min before use.
2) Keep the arc as short as possible .
3)Adopt back step method or strike the arc on a small plate prepared for this particular purpose because ar stricking on the base metal is in danger of initing cracking.

Chemical Composition Of Weld Metal

C% Mn% Si% S% P% Ni%
0.090 Max 1.60 Max 0.30 Max 0.030 Max 0.030 Max 1.50 Max

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²) Y.S.(N/mm²) ELONGATION ( L = 4d ) % IMPACT (CVN) AT – 50º C( J ) Hydrogen(Mercury method) in 100grm weld meta
520 Min 450 Min 22 % Min 40 Joules Min 5 ml (Max)

Packing and Welding Current

SIZE ( mm ) PIECES PER PACKET PIECES PER CARTON Current (Amps) In Amps
2.50 X 350 5 20 AC/DC (+) 70 – 90
3.15 X 350 5 20 90-130
4.00 X 350 5 20 140-180
5.00 X 350 5 20 180-230

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS: SFA 5.11, E NiCrMo-6 EN ISO 14172 A E Ni 6620