Welding Electrode

ROYAL CHROME – 1 MOD (E 8018-B2)

E 8018-B2

AWS : SFA 5.5, E 8018-B2

Applications

Joining of crack resistant steels, low alloy steels. Welding on equipment of Oil reneries, pipeline & high temperature synthetic chemical industries. Electric power plant.

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Preheat at 150 – 250 °C and post heat at 690 ± 15 °C.
2) Dry the electrode a 250 – 300 °C for 60 Min- before use .
3) Keep the arc as short as possible.

Chemical Composition Of Weld Metal

C% Mn% Si% S% P% Cr% Mo%
0.05- 0.12 0.90 Max 0.80 Max 0.010 Max 0.015 Max 1.0 – 1.50 0.40 – 0.65

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²) Y.S.(N/mm²) ELONGATION ( L = 4d ) % IMPACT(CVN) AT – 18° C ( J ) Hydrogen(Mercury method) in 100grm weld meta
550 Min 460 Min 19 % Min 27 Joules Min 5ml Max

Packing and Welding Current

SIZE ( mm ) KG PER PACKET KG PER CARTON Current (Amps) In Amps
2.50 X 350 5 20 AC/DC (+) 70 – 100
3.15 X 350 5 20 100-140
4.00 X 350 5 20 140-180
5.00 X 350 5 20 180-230