It is used for welding of 18% Cr, 12% Ni & 2.50% Mo steel also use for welding of AISE 316L & 317L type of stainless steel in chemical plant, paint, pulp paper & textile industries,CF-8M,CF-3M
1G 2F 3G 4G
15-20mm
Carbon Dioxide (CO2) shielding
Gas Flow:15-20 Lit/Min.
15 kgs. Vaccum packed plastic spool
Element | C% | Mn% | Si% | S% | P% | Cr% | Ni% | Mo% | Cu% |
---|---|---|---|---|---|---|---|---|---|
Typical Values | 0.040 | 0.50-2.50 | 1.0 Max | 0.030 Max | 0.040 Max | 17-20 | 11-14 | 2.0-3.0 | 0.75 Max |
U.T.S (N/mm²) | ELONGATION ( L = 4d ) % |
---|---|
485-580 Min | 30-38 Min |
Diameter(mm) | Flat & Horizonta (A) | Flat & Horizontal (V) | Vertical – Up(V)) | Vertical – Up(V) | Overhead(V) | Overhead(V) |
---|---|---|---|---|---|---|
1.20 | 160-210 | 26-30 | 120-160 | 22-26 | 150-180 | 26-30 |
1.60 | 190-250 | 26-30 | 160-200 | 22-27 | 180-210 | 26-30 |