Welding Electrode

Welding Positions

1G 2F 3G 4G 5G

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS : SFA 5.5, E 7018 B2L EN ISO 3580 A E CrMo 1 L B 32 H5
AWS: SFA 5.11, E Ni -1 EN ISO 14172 A E Ni 2061
AWS / SFA 5.11 E NiCrMo – 3 EN ISO 14172 A E Ni 6625