Welding Electrode

Applications

Cutting and piercing of steel, cast iron, copper Alloy, aluminum. Excellent for burning quirets, Dismantling site and for cutting out unwanted Metal in foundry castings.

Welding Positions

1G 2F 3G 4G 5G

Notes on Usage

The electrode is inclined to the surface at 35 o Angel . the arc is pushed deeper and forward to drive the molten metal and slag
on words. For deeper groove repeat procedure in stages until the required depth is reached.

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONIn Amps
3.15 X 3502 Kg10 Kg250 – 350
4.00 X 3502 Kg10 Kg300 – 400
5.00 X 3502 Kg10 Kg350 – 500

Related Products

1) Redry electrode at 250 °C for 2 hours. Keep the arc as short as possible.
AWS : A / SFA 5.11, E Ni Cu - 7 EN ISO 1472 A E Ni 4060
AWS / SFA 5.11 E NiCrMo – 3 EN ISO 14172 A E Ni 6625