Welding Electrode

ROYAL THERM (E 7018)

AWS : A 5.1, E 7018

Applications

Ship Building, Pipelines, Bridges, Boilers, Pressure Vessels, Restrained Joints, Penstocks, Blast Furnace Steel Work, Atomic Reactor Shell & Pipework.

Approvals

L.R.S, I.R.S, I.B.R, P.D.I.L, B.V., B.I.S. [ISI], E.I.L, TOYO [TEIL], RPL-BECHTEL, THERMAX, L & T, I.P.C.L, K.PG.I.L, I.O.C.L, M.R.P.L, M.M.D., UDHE INDIA LTD. , B.H.E.L., B.H.P.V., ABS, DNV, NPCIL, M.N.DASTUR & CO., RDSO CLASS A4 B2, SUZLON ENERGY, TPL

Welding Positions

1G 2F 3G 4G

Notes On Usage

1) Dry the electrode a 300-350 °C for 60 Min- before use .
2) Keep the arc as short as possible
3) Use wind screen against strong wind.

Chemical Composition Of Weld Metal

C%Mn%Si%S%P%Cr%Ni%Mo%
0.15 Max1.60 Max0.75 Max0.035 Max0.035 Max0.20 Max0.30 Max0.30 Max

Mechanical Properties Of Weld Metal

U.T.S.(N/mm²)Y.S.(N/mm²)ELONGATION( L = 4d ) %IMPACT (CVN) AT – 30° C ( J )RADIOGRPHY TESTHydrogen content in 100grm weld metal
490 Min400 Min22 % Min27 Joules MinSatisfactory as per IIW blue std5 ml Max

Packing and Welding Current

SIZE ( mm )KG PER PACKETKG PER CARTONCurrent (Amps)In Amps
2.50 x 350520AC 70 OCV/DC+60 – 95
3.15 x 35052090 – 120
4.00 x 350520140 – 190
5.00 x 350520190 – 250
6.30 x 450520250 – 310

Related Products

AWS: SFA 5.11, E NiCrFe-2 EN ISO 14172 AE Ni 6082

Share On:

Enquiry form

Contact Form